THE COURSE / M10 MEMORY / M10.6
Stacking: MR-MUF
After this lesson you can:
- Follow a stack from tacking its dies to joining every bump at once and moulding it.
- Explain what MR-MUF trades against bonding with film, TC-NCF.
- Say why hybrid bonding is the next step for taller stacks.
Loading the lesson…
Sources
- K.-M. Harr (SK hynix), "SK hynix's MR-MUF Innovations Tackle Heat Generation to Secure HBM Leadership," EE Times, 18 December 2024. Mass reflow connects stacked chips by melting the bumps between them, all layers heated at once; TC-NCF instead applies a film after each chip is stacked, heat and pressure melting it to glue them; EMC, a thermosetting polymer, fills the gaps; MR-MUF since 2019 (HBM2E), 36% more heat dissipation than HBM2; Advanced MR-MUF from 2023, its EMC 1.6 times as conductive; up to four times the thermal dummy bumps of TC-NCF; 12-high chips 40% thinner than 8-high; warpage from pressure and thin chips a pressing issue.
- SK hynix, "SK hynix Begins Volume Production of the World's First 12-Layer HBM3E," 26 September 2024. 36 GB in 12 layers; each DRAM chip made 40% thinner, so the stack keeps the eight-layer product's thickness; 9.6 Gbps; TSVs link upper and lower chips through thousands of fine holes; Advanced MR-MUF injects liquid protective material between the chips, controls warpage, reduces the pressure on the stacked chips, and dissipates 10% more heat than the previous generation.
- SK hynix, "SK hynix Ships Samples of 12-Layer Next-Gen HBM4E," 18 June 2026. 48 GB in a 12-layer stack, up to 16 Gbps a pin, Advanced MR-MUF.
- JEDEC, "JEDEC and Industry Leaders Collaborate to Release JESD270-4 HBM4 Standard," 16 April 2025 (as reprinted by StorageNewsletter, 17 April 2025). HBM4: transfer speeds up to 8 Gb/s across a 2048-bit interface, total bandwidth up to 2 TB/s a stack; 32 channels a stack, up from HBM3's 16, each with two pseudo-channels; 4-, 8-, 12- and 16-high stacks of 24 Gb or 32 Gb dies, to 64 GB; backwards compatible with HBM3 controllers.
- PSK Holdings, Investor Relations book (English, 2025). The ECOLITE series for descum and surface treatment in wafer- and panel-level packaging: descum removes residual scum after lithography, critical for RDL profiles and bump shapes; surface treatment removes residue or metallic ions and improves adhesion. GENEVA, the world's first system to mass-produce fluxless reflow, for plating bump reflow and bonding, including HBM and 2.5D packaging; SEMIgear (US) acquired in 2012.
- Lam Research, SABRE 3D (product page, read 1 November 2026). Electroplating for wafer-level packaging and filling TSVs, at the scale of microns rather than the angstroms of BEOL damascene, so long deposition times and multi-step processing; key applications TSV, copper pillar, RDL and Cu/SnAg and Ni/Au microbumps.
- EV Group, "Hybrid and Fusion Bonding" (technology page, read 25 October 2026). Fusion, or direct, bonding joins dielectric layers on each wafer: activated surfaces pre-bond at room temperature through hydrogen bridge bonds, and an anneal turns them covalent. Hybrid bonding adds metal pads in the interface for face-to-face electrical connection, as in stacked image sensors, memory and 3D systems-on-chip.
- Besi, Datacon 8800 CHAMEO ultra plus AC (product page, read 1 November 2026). Besi's hybrid bonding platform: 100 nm alignment at 3 sigma; up to 2,000 cycles an hour (dry); hybrid bonding needs the highest cleanliness, an ISO 3 atmosphere in the working area; in-situ IR inspection of placement.