THE COURSE / M11 PACKAGE AND TEST / M11.3
Bumps and flip chip
After this lesson you can:
- Say why a big chip is flipped: connections over its whole face, short and many.
- Follow a copper pillar from its seed and resist through plating, strip and reflow.
- Follow a flip-chip die onto its substrate: flux, place, reflow, wash, underfill, cure.
Loading the lesson…
Sources
- Wikipedia, "Flip chip" (read 3 November 2026). Solder bumps deposited on the chip pads in the last wafer step; the chip flipped face down, aligned to the matching pads, and the solder reflowed: controlled collapse chip connection, C4, brought to market by IBM in the 1960s; the short connections greatly reduce inductance and conduct heat better; the underfill distributes the thermal expansion mismatch between chip and board, preventing stress concentration in the joints.
- M. J. Lee (Altera), S. Park, D. Ryu, M. Lee (Amkor), H. Saiki, S. Mori, M. Nagai (NTK), "Packaging Technology and Design Challenge for Fine Pitch Micro-Bump Cu-Pillar and BOT Using TCNCP," IPC APEX EXPO 2015. Copper pillar bumps are gradually taking the place of solder bumps in flip chip, especially below 150 to 130 µm pitch, down to 40 µm: a copper column with a tin-silver solder cap plated on top; better fatigue life, electrical performance and fine-pitch assembly; finer pitch raises current density and the risk of electromigration, which copper withstands; fewer bridges than solder; test bumps 30 µm across and 40 µm tall.
- Canon, FPA-5520iV and its options (product page, Japanese, read 3 November 2026). An i-line (365 nm) stepper for advanced packaging on 300 mm wafers, at 1:2 reduction: the base model resolves 1.5 µm or finer over a 52 x 34 mm field (0.8 µm with the HR option), overlay 0.15 µm; the LF options a 52 x 68 mm field; about 20% more throughput than the FPA-5510iV for thick resist.
- ACM Research, Ultra ECP ap (product page, read 3 November 2026). Electroplating for advanced packaging on 200 and 300 mm wafers: copper via fill, copper pillar bumping, nickel and tin-silver; 16 to 20 plating chambers for copper, tin-silver and nickel, each anode in its own membrane-isolated chamber; within-die and wafer-to-wafer uniformity under 3%; 30 wafers an hour for pillars.
- Indium Corporation, "Reflow of copper pillar microbumps" (blog, read 3 November 2026). Plated copper pillars with solder end caps are reflowed so the cap is smooth, hemispherical and free of residue; after the resist strip, the rough plated cap carries tin oxides and hydroxides and trapped organics.
- Besi, Datacon 8800 FC QUANTUM advX (product page, read 3 November 2026). A flip-chip bonder for FC-BGA, FC-CSP, DRAM and fan-out chip-to-wafer: dies 0.3 to 40 mm, 50 µm to 3 mm thick; placed to ±4 µm at 3σ (±3 µm option); up to 10,000 an hour; bond force 2 to 50 N; flux dipping; substrates in boats, strips or a wafer in a carrier.