THE COURSE / M11 PACKAGE AND TEST / M11.8

The accelerator

After this lesson you can:

  • Follow the module onto its substrate, under its lid, and onto its balls.
  • Explain why a big package warps, and why it is measured through the reflow profile.
  • Say what system-level test adds, and why the whole build's yield is a product of every step's.

Loading the lesson…

Sources

  1. Wikipedia, "Flip chip" (read 3 November 2026). Solder bumps deposited on the chip pads in the last wafer step; the chip flipped face down, aligned to the matching pads, and the solder reflowed: controlled collapse chip connection, C4, brought to market by IBM in the 1960s; the short connections greatly reduce inductance and conduct heat better; the underfill distributes the thermal expansion mismatch between chip and board, preventing stress concentration in the joints.
  2. US 2015/0069089 A1 (TSMC), "Lid attach process and apparatus for fabrication of semiconductor packages" (2015). A thermal interface material wet-dispensed on top of the die, a seal adhesive on the substrate's periphery, and a lid of thermally conductive copper or aluminium lowered onto both to encapsulate and protect the die; heat cures the structure.
  3. Wikipedia, "Thermal interface material" (read 3 November 2026). Any material inserted between two components to enhance the thermal coupling between them; common metal TIMs are soft, compliant indium alloys; thermal pastes give a very thin bond line.
  4. Wikipedia, "Ball grid array" (read 3 November 2026). Solder balls on the package's pads, held by a tacky flux, melted in a reflow oven; low thermal resistance and lead inductance; bending from the difference in thermal expansion between package and board can fracture the joints.
  5. Akrometrix, FAQ (read 3 November 2026). Shadow moiré and digital fringe projection measure warpage full-field, an out-of-plane displacement for every pixel; samples from 2 x 2 to 600 x 600 mm; sub-micron resolution up to 20 mm, 2.5 µm larger; room temperature to 300 °C, or down to -55 °C; heating and cooling at 1 to 3.5 °C/s, following reflow and cure profiles.
  6. Advantest, 7038 Single Test Rack system-level test and burn-in (news release, 18 September 2025). Extends the 7038 system-level test platform: liquid cooling of up to 1.4 kW per test site, where air-cooled systems are limited to about 100 W per device; for AI, HPC and automotive devices, so they perform as designed in real-world use.
  7. Y. Han, H. Xu, M. Lu, H. Wang, J. Huang, Y. Wang, Y. Wang, F. Min, Q. Liu, M. Liu and N. Sun, "The Big Chip: Challenge, model and architecture," Fundamental Research 4, 1431–1441 (2024). The largest single die, 858 mm² (26 × 33 mm), set by the reticle and optics; the Poisson model tends to underestimate large chips' yield; the negative binomial model is widely used; a multi-chiplet system's yield set by its chiplets' yields and the bonding yield, which falls as chiplets are added.