THE COURSE / M2 PURE SILICON / M2.2
Growing the crystal
After this lesson you can:
- Describe a Czochralski puller and how one crystal is drawn from a melt of polysilicon.
- Explain why the crystal starts with a thin neck, and name its neck, shoulder, body and tail.
- Explain why the dopant and the oxygen change along the ingot, and what a magnetic field and float zone are for.
- Explain why a puller is stripped and its parts baked clean after each pull, and how its argon is recovered.
Loading the lesson…
Sources
- SUMCO, Production processes (read 4 November 2026). Polysilicon purified until its metal impurities are no more than a few parts per billion goes into a quartz crucible with minute amounts of boron or phosphorus to set the resistance, and is melted at around 1420 °C; a seed crystal is placed on the melt and pulled up while rotating, giving a monocrystalline ingot with the seed's orientation. MCZ applies a strong magnetic field; FZ makes ingots at low oxygen without a quartz crucible. The ingot is ground to a uniform diameter and sliced about 1 mm thick, lapped with alumina, etched, polished with colloidal silica, cleaned and inspected.
- PVA TePla, SC-32 product overview (brochure, version 09/2026, read 4 November 2026). Crystals up to 310 mm for 12" wafers, removable length up to 3,600 mm; charge up to 500 kg (customer hot zone) or 420 kg (PVA's); crucibles up to Ø 812 mm (32"); process chamber Ø 1,250 mm, three or five segments; polysilicon melted in argon by a resistance heater (melting point around 1,412 °C); a rotating seed dipped in, a slight temperature drop starts crystallization, pulling rate and temperature regulated for a constant diameter; crystal drive 0.05–560 mm/min and 0.1–20 rpm, crucible drive 0.05–200 mm/min and 0.1–20 rpm; single or dual camera systems, a stereo camera system in PVA's hot zone set; optional transversal or CUSP magnet up to 0.4 T; about 30,000 kg without the magnet; about 280 kVA and 300 l/min of cooling water.
- US 2003/0047130 A1, "Process for eliminating neck dislocations during Czochralski crystal growth" (background, read 4 November 2026). Dislocations are generated by the thermal shock of the seed touching the melt and spread through the crystal unless removed in the neck; the conventional Dash neck is 2 to 4 mm across, grown at up to 6 mm/min, and is free of them after about 100 to 125 mm; the neck is the crystal's weakest part, so Dash-necked crystals were typically grown to 100 kg or less; a wider neck needs a larger seed, makes more dislocations and takes 175 mm or more to clear them.
- Wikipedia, Czochralski method (read 4 November 2026). Jan Czochralski's method, 1916 at AEG (1915 in the article's lead); revived for semiconductors by Gordon Teal at Bell Labs after the Second World War; grown in argon from a high-purity quartz crucible; the crucible dissolves into the melt, so Czochralski silicon holds about 10¹⁸ oxygen atoms per cm³, whose precipitates can trap metal impurities (gettering) and which strengthens wafers by pinning dislocations; an impurity in the solid follows C = k C₀ (1 − f)^(k − 1), k the segregation coefficient.
- Oxygen transport during Czochralski silicon growth, Heliyon (2024) (introduction, read 4 November 2026). Oxygen in Czochralski silicon comes from the dissolving quartz crucible; the rest of it, besides what the crystal takes up, evaporates at the free surface, where the melt meets the argon; oxygen affects the melt's heat transfer and the crystal's growth, and in solar cells degrades them.
- PVA TePla, Float zone (read 4 November 2026). A polysilicon rod over a high-frequency induction coil; its lower end melts without contact, a seed touching the molten zone is pulled down slowly as the rod feeds in; no quartz crucible, only a small section heated; purities up to 11N and significantly lower oxygen than crucible methods; for power devices (diodes, thyristors, IGBTs, MOSFETs); the FZ-35 grows crystals up to 200 mm.
- SUMCO, JP2024073310A, collecting dust while a puller's crucible and heater cool (read 9 November 2026). During the pull the crucible's oxygen and the melt make silicon oxide, SiOx, which vaporises, moves with the inert gas, cools and solidifies on the main chamber's walls and its parts, such as the heater, building up over time. After the pull the puller is dismantled and cleaned in the clean room, the crucible's leftover silicon removed and the crucible changed; prior art covers the chamber with plastic sheet, a supply fan and a suction hood to an exhaust fan with a HEPA filter in a pit below the floor. The crucible and heater are around 200 °C when the furnace is opened, and are left to cool to about 50 °C or below.
- SUMCO, JP2021042103A, regenerating a puller's parts (read 9 November 2026). SiO, SiO2 and metallic silicon evaporate from the melt's surface and solidify on parts such as the heat shield and the flow tube; flakes that fall into the melt become impurities and worsen the crystal, and a quartz flow tube turns brown and blocks the view in. The applicant's method: heat the parts, in an apparatus that uses a silicon single-crystal puller, under inert gas at 2.67 kPa (20 torr) or less, the surface at 1,700 °C or more (sublimation starts at about 1,000 °C) and below where the part deforms, for at least two hours; the sublimed silicon leaves with the gas.
- Shin-Etsu Handotai, JP2015020928A, pretreating a puller's exhaust argon for recovery (read 9 November 2026). As single-crystal production grows, so does the argon used, and recovering and reusing the pullers' exhaust argon is an important way to cut costs. Its silicon oxide is dissolved by contact with a strong alkali solution, and the alkaline mist is taken out by a demister.
- Shin-Etsu Handotai, JP2015140281A, recovering and purifying argon from pullers (read 9 November 2026). Waste argon pumped from the pullers by vacuum pumps, with nitrogen, oxygen and carbon monoxide, into a holding tank; solids removed; the oxygen turned to water and the carbon monoxide to carbon dioxide on catalysts placed inside a two-stage compressor, by the compression heat alone; the water taken by a dryer first, then the nitrogen and carbon dioxide adsorbed in room-temperature adsorption towers.