From ingot to wafer
After this lesson you can:
- Follow an ingot through forming: cropped, ground round, notched, sliced by wire, edge-ground, ground flat and etched.
- Explain how a slurry wire saw cuts, why the cut itself costs silicon, and how the grit goes round again while the kerf leaves as waste.
- Explain why every mechanical step leaves damage, and why the last of it is etched away.
Loading the lesson…
Sources
- SUMCO, Production processes (read 4 November 2026). Polysilicon purified until its metal impurities are no more than a few parts per billion goes into a quartz crucible with minute amounts of boron or phosphorus to set the resistance, and is melted at around 1420 °C; a seed crystal is placed on the melt and pulled up while rotating, giving a monocrystalline ingot with the seed's orientation. MCZ applies a strong magnetic field; FZ makes ingots at low oxygen without a quartz crucible. The ingot is ground to a uniform diameter and sliced about 1 mm thick, lapped with alumina, etched, polished with colloidal silica, cleaned and inspected.
- Daitron, CVP wafer contouring vertical polisher (read 6 November 2026). CVP-320: notch wafers, 12 or 8 inch; two stations; horizontal coarse grinding (metal-bonded, 100 mm, option), vertical contouring (resin-bonded, 60 mm), notch grinding (option); profile measurement; washing unit.
- Shin-Etsu Handotai, US 8,286,623 B2, "Band saw cutting apparatus and ingot cutting method" (background, read 4 November 2026). The ingot's cone-shaped top and tail are cut away to separate the cylindrical body, which is cut into blocks as needed and then processed into wafers; band saws are used more as wafers grow larger.
- Freiberg Instruments, Ingot XRD (read 4 November 2026). Determines an ingot's crystal orientation by X-ray in under 5 s, on-axis to 0.005°; optically finds the flat or notch on raw or ground ingots (notch position to under 0.01°, depth under 6 µm); glues the end pieces and marks the ingot; ingots 70 to 300 mm across, up to 520 mm long.
- Wikipedia, Wafer (electronics) (read 4 November 2026). Ingots are sliced with a wire saw, machined flat, etched to remove crystal damage, and polished. 300 mm wafers are 775 µm thick. Wafers under 200 mm have flats showing the crystal planes; 200 mm and larger use a single small notch. Edge rounding prevents stress concentrations and chipping.
- Komatsu NTC, Wire saws (read 4 November 2026). MWM3050nQ: workpiece up to Φ300 × L450 mm, one at a time, slurry; 2,000 × 3,550 × 3,500 mm. Its ND200 and ND660 cut with diamond wire: "reduced material loss due to finer wire by adopting diamond wire."
- T. Behm, W. Fütterer, C. Funke, S. Kaminski, H.J. Möller, R. Rietzschel, T. Wagner (TU Bergakademie Freiberg), "Challenges of the wire saw wafering process", Photovoltaics International, 11th edition (February 2011). Multi-wire sawing is the main slicing technique for large crystals in photovoltaics and microelectronics. Slurry is poured above the wire web, which drags it to the ingot, fed at 0.4 to 0.8 mm/min; the wire moves at up to 15 m/s. Free SiC particles in a carrier fluid, mostly polyethylene glycol, remove material by rolling and indenting into the silicon and chipping it away; the gap under the wire is about 10 to 16 µm, set by the bigger particles (a 120 µm wire in their model experiment). The damage is a rough surface and microcracks reaching into the bulk; finer grit makes less.
- Fraunhofer IWM, SimPARTIX: Wire sawing of silicon wafers (read 4 November 2026). A steel wire guided over grooved rollers keeps the wires evenly spaced; the ingot is pressed against them, wetted with slurry of polyethylene glycol and angular SiC grains. Kerf loss is set mainly by the wire's diameter and the grains' sizes, and by feed rate and wire tension; for solar wafers about half the silicon is cut away.
- G. Zhang, B. Liu, J. Zhao, W. Chen, J. Wang, Q. Zhou, H. Tu (GRINM, Beijing), "Study on geometry, surface damage and rapid thermal annealing of 300 mm as-cut silicon wafers", Electrochemical Society meeting abstract MA 201, 565. The damage layer of 300 mm wire-sawn wafers was about 11 µm deep and uniform; inner-diameter-sawn wafers about 22 µm, deeper and less even. A wire-sawn surface resembles a lapped one, since both are free-abrasive machining. Wire saw is the more suitable for large diameters.
- Shin-Etsu Handotai, JP2011005561A, recycling wire-saw slurry (read 8 November 2026). The line: spent slurry from the saw to the primary decanter, whose cake, mainly reusable abrasive, goes to the blending tank and whose liquid goes by its tank to the secondary decanter; that one separates waste sludge from a liquid, mainly coolant, which goes to blending. A new slurry tank adds new abrasive and coolant; blended slurry goes by the reclaimed slurry tank and a day tank to the saw's nozzle. Example: both decanters Ishikawajima's HS-205L, the primary at 400 G, the secondary at 3000 G. The patent's own proposal, distilling and classifying the sludge, is not taught.
- Shin-Etsu Handotai, JP2016135529A, a wire saw's slurry temperature (read 8 November 2026). A Komatsu NTC wire saw; 130 µm high-tension steel wire at 25 N, from a supply reel to a take-up reel; GC #2000 slurry, coolant and abrasive 50/50; a slurry tank with a slurry chiller; supplied at 24.0 °C at the start and end of the cut and 18.1 to 22.0 °C in the middle, in the examples.
- IHI, Wire-saw Slurry Recycle System (WSRS) catalogue (read 8 November 2026). Two-step separation; 3,000 to 15,000 L a day; 13 × 5 × 7 m and 27 t empty at 8,000 L a day. Recovery: abrasive 80 to 95%, coolant 60 to 90%, silicon removed 30 to 60%, the coolant with vacuum distillation or filtration. More than 70% lower running cost, IHI's estimate.
- JTEKT, DXSG320 wafer grinding (read 4 November 2026). Grinds both faces of silicon wafers at once, from as-sliced to ±1 µm; 200 and 300 mm; about 90 s a 300 mm wafer; 1,900 × 2,560 mm, 5,000 kg.
- SUMCO, US 7,851,375 B2, "Alkaline etchant for controlling surface roughness of semiconductor wafer" (background, read 4 November 2026). Etching removes the damage layer left by block cutting, outer grinding, slicing and lapping. Acid etchant: hydrofluoric and nitric acids diluted in water or acetic acid; the nitric acid oxidises silicon to SiO₂, which the hydrofluoric acid dissolves. Alkaline etchant: potassium or sodium hydroxide in water. After lapping, an acid etch of, for example, 20 µm a side, 40 µm or so in all; mirror polishing then removes, for example, 10 µm.