After this lesson you can:

  • Follow a wafer through finishing: marked, polished on both faces, edge-polished, final-polished, cleaned, measured and boxed.
  • Explain why polishing runs from hard and heavy to soft and light, and what each stage is for.
  • Say what proves a wafer good: its flatness, site by site, and its count of light points.

Loading the lesson…

Sources

  1. SUMCO, Production processes (read 4 November 2026). Polysilicon purified until its metal impurities are no more than a few parts per billion goes into a quartz crucible with minute amounts of boron or phosphorus to set the resistance, and is melted at around 1420 °C; a seed crystal is placed on the melt and pulled up while rotating, giving a monocrystalline ingot with the seed's orientation. MCZ applies a strong magnetic field; FZ makes ingots at low oxygen without a quartz crucible. The ingot is ground to a uniform diameter and sliced about 1 mm thick, lapped with alumina, etched, polished with colloidal silica, cleaned and inspected.
  2. SUMCO, US 12,083,624 B2, "Method of printing laser mark and method of producing laser-marked silicon wafer" (background and description, read 5 November 2026). After beveling and lapping or grinding, the periphery of the front or back surface may be printed by laser with an identification code made of dots; then etching and polishing, final cleaning, inspections, and wafers that meet the standards are shipped. A dot from one shot is about 2 to 10 µm deep. Strain around the dots spoils the periphery's flatness after polishing; ultraviolet light (355 nm or less) reduces it.
  3. InnoLas Semiconductor, IL 3000 (read 5 November 2026). Hard laser marking of 300 mm wafers, particularly unpolished; front, back or both; up to 4 open cassette stations; up to 125 wafers an hour (SEMI M12 and T7); marking accuracy about ±100 µm.
  4. Siltronic, US 8,376,811 B2, "Method for the double sided polishing of a semiconductor wafer" (background and description, read 5 November 2026). In DSP, wafers in the recesses of metal or plastic carrier plates move on a set path between two rotating polishing plates covered with polishing pads, in a polishing sol; the final nanotopology is made by polishing, and polishing both sides at once was developed to improve planarity. Besides DSP, CMP of the device side only, with a softer pad, removes defects and roughness: finish polishing. The AC2000 from Peter Wolters, Rendsburg, is such a machine; its pin rings drive the carriers on a planetary path; a typical carrier holds three wafers, with inlays to protect their edges, including from metals released from the carrier. Glanzox 3900 (Fujimi): pH 10.5, about 9 wt% colloidal SiO₂, 30 to 40 nm. Nanotopology per SEMI: deviation over spatial wavelengths 0.2 to 20 mm in the fixed quality area, as peak to valley in windows such as 2 × 2 mm.
  5. SUMCO, US 7,338,904 B2, "Method for manufacturing single-side mirror surface wafer" (read 6 November 2026). Uses a double side polishing machine (LPD300) made by Fujikoshi, with no sun gear, on 300 mm silicon wafers: one carrier plate with five holes spaced every 72°, moved by four eccentric arms in a circular motion in the horizontal plane without turning on its own axis, each wafer revolving within its hole; each platen has its own motor.
  6. Shin-Etsu Handotai, US 6,729,941 B2, "Process for manufacturing semiconductor wafer and semiconductor wafer" (background and example, read 5 November 2026). Slicing, chamfering, lapping, etching, polishing, cleaning. Polishing runs from rough (for planarisation, a hard non-woven cloth impregnated with urethane) to final (for roughness and scratches, a suede-like cloth), in silica dispersed in alkaline solution; prior-art removals of 5 µm or more, 0.1 µm or more and 0.01 µm or more. Example: first polish 6–10 µm; final polish on suede at 80–120 g/cm², colloidal silica, 0.05 µm, with no cloudiness.
  7. SpeedFam, Edge Polisher (read 7 November 2026). EP-300-X for 300 mm prime wafers: three-surface polishing of the upper and lower bevels and the apex; orientation flat and notch region mirror polishing; about 550 edge polishers shipped since 1988; the global standard in prime wafer factories, in SpeedFam's words.
  8. Shin-Etsu Handotai, JP2006-237055 (read 7 November 2026). SpeedFam's type IV mirror chamfering machine: the wafer held on a chuck, tilted and pressed against a rotating drum faced with a SUBA400 pad; silica slurry at pH 11, 2 L/min; a load of 2.0 kgf.
  9. Pre-Tech and Shin-Etsu Handotai, JP2010-258084 (read 7 November 2026). A batch megasonic cassette-less cleaner on mirror-polished 300 mm wafers: SC-1 at 1:1:10, 50 °C, 1 MHz, ten minutes; five baths with a robot arm between them, DIW in all but the second bath, in a second example.
  10. Pre-Tech, Cassette-less Wafer Cleaning System (read 7 November 2026). Consistent cleaning where a cassette would touch the wafer; less chemical in a bath and carried between baths; FINE-SONIC megasonics; transfer robot, baths, loader, unloader, piping.
  11. SCREEN, Wet Station FC-3100 (read 5 November 2026). 1,000 wafers an hour; seven independent modules, dual cleaning baths in a module; HiLPD low-pressure drying with high-concentration IPA vapour, which greatly suppresses watermarks.
  12. W. Kern and D. A. Puotinen, "Cleaning solutions based on hydrogen peroxide for use in silicon semiconductor technology," RCA Review 31, 187–206 (1970). The RCA clean: water, peroxide and ammonia (5-1-1 to 7-2-1) for organics and some metals, then water, peroxide and hydrochloric acid (6-1-1 to 8-2-1) for heavy metals, each 10 to 20 minutes at 75 to 85 °C; safe for silicon and oxide while peroxide remains.
  13. KLA-Tencor, US 7,324,917 B2, "Method, system, and software for evaluating characteristics of a surface with reference to its edge" (background, read 5 November 2026). Wafer makers and chip makers need flatness, thickness, bow and warp, used in lithography. SEMI M1 and MF1530: flatness of the front as it would be with the back ideally flat, as on a clean flat chuck; the fixed quality area inside an edge exclusion, commonly 2–3 mm (2004); sites such as 26 × 8 mm; SFQR: by site, front reference, least-squares plane fitted in the site, reported as the range.
  14. SUMCO, US 8,379,196 B2, "Method for judging whether semiconductor wafer is non-defective wafer by using laser scattering method" (background, read 5 November 2026). Wafer makers and device makers judge a wafer good or not from the number of light point defects (LPDs) found by laser scattering; an LPD's size is given from the scattering of a polystyrene latex (PSL) standard particle; the detection limit required is below 65 nm (2009); haze is the background signal, from microroughness.
  15. SUMCO, US 10,526,728 B2, "Silicon wafer and method for manufacturing same" (background, read 5 November 2026). A spot of laser light in the visible to ultraviolet is moved across the rotating wafer; defects show as light points (LPDs); some are protrusions, some concavities.
  16. Miraial, 300 mm FOSB (read 6 November 2026). KT-3004A-4: 327 long × 389.5 wide × 341.8 mm high; body and door polycarbonate, groove plates PBT; to SEMI M31, E1.9, E47.1, E15.1, E57 and E62.
  17. Entegris, SB300 FIMS compatible FOSB data sheet (read 5 November 2026). 25 wafers of 300 mm at 10 mm pitch; ultrapure polycarbonate shell and door; metal-free assembly; FIMS automated door, kinematic coupling; protective gasket and filter; 389.52 × 332.77 × 336.93 mm; 4.6 kg empty, 7.8 kg full.
  18. SUMCO, CSR reports 2016 and 2020 (read for the plan, November 2026). SUMCO ships 300 mm wafers in reusable containers: 61.4% of them in 2014 (the 2016 report), 63.2% in 2019 (the 2020 report).
  19. Shin-Etsu Handotai, JP2004281978A, an automatic washer for wafer shipping boxes (filed 2003, read 9 November 2026). Used boxes get dirty inside and out and can contaminate the wafers, so they are cleaned before wafers are loaded. Taken apart into body, upper lid, inner box, retainer and gasket, the parts ride a mesh belt under a top net through pre-wash in warm pure water, about 0.1% of a commercial surfactant, warm high-purity rinses, a drain by clean dry air at about 30 to 100 °C and a heated, reduced-pressure dry: about 100 boxes an hour, against about 20 on a commercial cleaner with racks.
  20. Entegris, SB300 FOSB for 300 mm wafers, user manual (read 5 November 2026). Protects wafers in 1.5 m drop tests; the all-plastic assembly prevents metallic contamination. SEMI M31: the FOSB ships 300 mm wafers from wafer suppliers to their customers, typically IC makers, who move them into a FOUP or open cassette; it is not used inside IC manufacturing.