THE COURSE / M2 PURE SILICON / M2.5
Engineered wafers
After this lesson you can:
- Explain what a polished wafer lacks for some chips: voids from the crystal near its surface, and one doping all the way through.
- Explain how epitaxy, an anneal in hydrogen or argon, and a buried layer under epitaxy each change the wafer, why a heavy wafer's back is sealed before epitaxy, and how heat kills oxygen's donors.
- Follow both routes to silicon on insulator, bonding and thinning, and Smart Cut's split, and say who orders which wafer.
Loading the lesson…
Sources
- SUMCO, Production processes (read 4 November 2026). Polysilicon purified until its metal impurities are no more than a few parts per billion goes into a quartz crucible with minute amounts of boron or phosphorus to set the resistance, and is melted at around 1420 °C; a seed crystal is placed on the melt and pulled up while rotating, giving a monocrystalline ingot with the seed's orientation. MCZ applies a strong magnetic field; FZ makes ingots at low oxygen without a quartz crucible. The ingot is ground to a uniform diameter and sliced about 1 mm thick, lapped with alumina, etched, polished with colloidal silica, cleaned and inspected.
- Sumitomo Mitsubishi Silicon (SUMCO), US 7,273,647 B2, "Silicon annealed wafer and silicon epitaxial wafer" (background, read 5 November 2026). COP defects, grown-in defects formed as the crystal grows, about 0.1 µm, at 10⁵ to 10⁶ per cm³; to reduce them a wafer is heated at about 1200 °C in a non-oxidizing atmosphere of hydrogen, argon or the like, which lowers their density in the surface layer and diffuses oxygen out, leaving neither oxygen precipitates nor COPs in the device region.
- Shin-Etsu Handotai, EP 1 632 591 A1, "Silicon epitaxial wafer, and silicon epitaxial wafer producing method" (background, read 5 November 2026). An epitaxial wafer's substrate is pulled by CZ, chamfered, sliced, lapped, etched and mirror-polished; silicon is then fed to it at high temperature to grow the layer by vapour phase epitaxy. A minute void in the CZ crystal that reaches the surface is a pit about 0.2 µm across, a COP (crystal originated particle); where one transfers to the epitaxial surface, the inspection counts it as a light point defect.
- Shin-Etsu Handotai, US 6,551,398 B2, "Heat treatment method for a silicon monocrystal wafer and a silicon monocrystal wafer" (background, read 5 November 2026). COPs are vacancy-type voids with a regular octahedral shape, introduced as the crystal grows; they are related to the time-dependent dielectric breakdown of oxide films. Hydrogen anneal reduces them; a typical condition is 1200 °C for 60 minutes, in a batch furnace, which etches about 0.5 µm of silicon, and some COPs remain.
- SUMCO, US 9,818,609 B2, "Epitaxial-silicon-wafer manufacturing method and epitaxial silicon wafer" (background and description, read 5 November 2026). An epitaxial film grown by CVD on a silicon wafer has, in theory, no oxygen. Latch-up: floating charges drive an unintended parasitic transistor, and the device may need powering off to recover; the p/p+ epitaxial wafer, an epitaxial film on a low-resistivity wafer doped heavily with boron, is used to prevent it. Grown at a target 1050 to 1280 °C, for instance from trichlorosilane, to 0.5 to 8.0 µm; the example 3 µm at about 1150 °C.
- SEH America, US 5,306,939 A, "Epitaxial silicon wafers for CMOS integrated circuits" (background, read 5 November 2026). A CMOS wafer: an epitaxial layer lightly doped with boron at 2×10¹⁴ to 2×10¹⁵ atoms/cm³ on a Czochralski substrate heavily doped at 3×10¹⁸, to reduce latch-up, which can start when the supply voltage is switched on. Heavy doping hinders measuring and precipitating the substrate's oxygen, but latch-up is so serious that most epitaxial CMOS wafers continue to be made on heavily doped substrates (filed 1990).
- SUMCO, JP2016213232A, an epitaxial wafer on a very low-resistivity substrate (read 8 November 2026). The steps: the back oxide, the oxide cleared from the rim (under 5 mm from the edge), an argon anneal, a prebake in hydrogen and hydrogen chloride, epitaxy. The back oxide by a continuous atmospheric-pressure CVD, Amaya Seisakusho's AMAX1200: monosilane and oxygen, 550 nm (100 to 1,500 nm), at 430 °C (400 to 450 °C); "by providing such a back oxide, autodoping is suppressed." Wafers doped with red phosphorus, about 0.7 to 0.9 mΩ·cm; epitaxy from trichlorosilane with phosphine at 1,060 °C, 4 µm, 0.3 Ω·cm.
- SUMCO, JP2025157587A, a silicon wafer and an epitaxial silicon wafer (read 8 November 2026). For power MOS transistors, a substrate of very low resistivity: 300 mm, phosphorus, 0.6 to 1.2 mΩ·cm. A back oxide by CVD, monosilane and oxygen, 100 to 1,500 nm at 400 to 450 °C, suppresses autodoping and the epitaxial layer's variation in resistance. The oxide can't be formed on the back alone: it forms on the bevelled edge too, and epitaxy over oxide may grow nodules, so the edge and the back's rim are cleared.
- Motorola, US 4,662,956, preventing autodoping of epitaxial layers (filed 1985). Autodoping: "undesired, uncontrolled doping of the epitaxial layer during growth"; out-diffusion from the doped substrate is the major contributor, the source of the dopant the back of the wafer, by diffusion through the gas. A thermally grown oxide on the back is considerably effective as a barrier, though not a complete one.
- M. Bruel (CEA), US 5,374,564 A, "Process for the production of thin semiconductor material films" (description, priority 18 September 1991, read 5 November 2026). Three stages: ions implanted through a face of the wafer make a layer of gas microbubbles in it, dividing the thin film above from the mass of the substrate; the face is put in intimate contact with a stiffener; heat treatment above the implanting temperature, above about 500 °C for hydrogen in silicon, rearranges the crystal and pressurises the bubbles, and the film separates from the substrate. Hydrogen is slowed mainly by ionisation, so few defects are made in the film and the bubbles sit near the depth of peak concentration, on a cleaving plane; moderate doses, for example 5×10¹⁶ cm⁻². A stiffener such as one with a 5,000 Å oxide.
- Soitec, Smart Cut technology (read 5 November 2026). Developed at CEA-Leti; light ion implantation and molecular adhesion bonding transfer ultrathin single-crystal layers from one substrate to another; the transferred layer's thickness is set precisely by the implantation energy; the donor substrate is refreshed and reused after each transfer; standard semiconductor tools; a range of top silicon and buried oxide thicknesses.
- Soitec, RF-SOI (read 5 November 2026). RF-SOI substrates for RF front ends (cellular, Wi-Fi, connectivity). RFeSI has four layers: top silicon for the devices, a buried oxide against parasitic capacitance, a trap-rich layer, and high-resistivity silicon. In 100% of 5G smartphones.
- Soitec, FD-SOI (read 5 November 2026). An ultra-thin film lets transistors run fully depleted; low active power and ultra-low leakage at very low supply voltages; used in wireless from IoT and smartphones to 5G mmWave.
- SUMCO, JP6988737B2, a silicon wafer whose thermal donors are held down (priority 2018, read 9 November 2026). Oxygen in the crystal is normally neutral, but in a heat treatment below about 600 °C a few to a dozen or so oxygen atoms gather into clusters that give up electrons: thermal donors. Treated above about 650 °C they return to neutral; that treatment is the donor killer anneal. Low-temperature steps in the device process can make them again, changing the resistivity or even reversing the conduction type.
- SUMCO, US 2007/0095274 A1, a silicon wafer and its production (priority 2005, read 9 November 2026). Supersaturated oxygen from the quartz crucible makes thermal donors, which can turn a wafer from p-type to n-type and sharply drop its resistivity; in low-resistance doped wafers their influence is minimal. Wafers are generally given a donor killer (DK) treatment against it; hydrogen- or argon-annealed wafers get it before the high-temperature anneal, for example 650 °C for about an hour.
- Mitsubishi Materials Silicon, US 5,449,883, continuous heat treatment against thermal donors (priority 1992, read 9 November 2026). The thermal donor should be killed before the wafer ships: after the rod is sliced and the wafers shaped and etched, a heat treatment, in the prior art 600 to 650 °C for 30 to 60 minutes; held around 700 °C for long, new donors form. Mitsubishi Materials Silicon is now part of SUMCO.