Skip to content

THE COURSE / M4 PATTERNING / M4.1

Print, then transfer

After this lesson you can:

  • Follow a layer through the patterning loop, from coating the resist to stripping it.
  • Use CD = k1·λ/NA to say what a wavelength and a lens can print.
  • Say why a sharper lens leaves less depth of focus, and why the wafer must be flat.

Loading the lesson…

Sources

  1. ASML, "The Rayleigh criterion," lithography principles (read 26 October 2026). CD = k1 · λ / NA: the critical dimension, the smallest possible feature; the wavelength; the numerical aperture, how much light the optics collect; k1, a coefficient set by many factors in the process. The physical limit is k1 = 0.25. Smaller features from a shorter wavelength, a larger NA, and k1 pushed toward its limit, by computational lithography among other tweaks.
  2. ASML, "Lenses and mirrors," lithography principles (read 26 October 2026). The highest-resolution DUV machines reach an NA of 1.35 by projecting through a layer of water between the lens and the wafer; without water, an NA above 1 was impossible. EUV is absorbed by most materials, so EUV systems use mirrors of over 100 layers, polished to less than an atom's thickness, the largest a metre across; High NA raised EUV's NA from 0.33 to 0.55.
  3. S. Hofman, "How immersion lithography saved Moore's Law," ASML (2 August 2023). In 2001 157 nm lithography hit problems; water under the lens extended 193 nm instead, with the same optics, masks and resists. The first immersion system announced in December 2003; volume production in 2006, NA from 0.93 to 1.2; then multi-patterning, where "overlay, rather than imaging resolution, became the critical parameter".
  4. A. Doolittle, ECE 6450, lecture 7, "Lithography and Pattern Transfer," Georgia Tech. The sequence: dehydration bake, adhesion promoter (HMDS), spin-coated resist, soft bake, exposure, post-exposure bake, develop. Spin: dispense slowly, then spin faster for the thickness and uniformity. Projection reduces the mask 4 to 10 times, shrinking mask defects too. Wmin = k·λ/NA; depth of focus ∝ λ/NA², so a planar surface matters. Lines: 436 (g), 365 (i), KrF 248 and ArF 193 nm; F₂ 157 nm never widely adopted.
  5. M. Östling, IH2655, lecture 9, "Microlithography," KTH (Spring 2013). R = k1·λ/NA and DOF = k2·λ/NA²; higher-NA lenses decrease the depth of focus. Resist contrast γ = 1 / log10(Df/D0): about 2–3 for DNQ resists, 5–10 for DUV; chemical amplification steepens the transition. Standing waves on reflective layers, suppressed by an anti-reflective coating; post-exposure bake smooths them. Soft bake 90–100 °C; develop 30 s to minutes.
  6. M. Hassaan, U. Saleem, A. Singh, A. J. Haque and K. Wang, "Recent Advances in Positive Photoresists: Mechanisms and Fabrication," Materials 17, 2552 (2024), CC BY. EUV light at 13.5 nm against DUV's 193 nm: each photon carries 14.3 times the energy, so there are fewer of them, and photon shot noise roughens lines under 10 nm. Wet resists are spin-coated.