A flat, clean back

After this lesson you can:

  • Say how the depth of focus is shared out, and how little of it the wafer's flatness gets.
  • Explain how a particle under the wafer spoils the pattern on top, and tell a wafer's particle from the chuck's.
  • Say why the back of a wafer is inspected and cleaned before it reaches the scanner.

Loading the lesson…

Sources

  1. R. Howland and M. Filzen (KLA-Tencor), "Process Watch: Exploring the dark side," Solid State Technology (2013). A back-side particle trapped between the chuck and the wafer causes a defocus defect, a hotspot, on the front: a particle of about 3 µm, or a cluster of smaller ones, raises the surface about 50 nm. At 28 nm, depth of focus is about 50 nm (193 nm, NA 1.35, k2 0.5), some 30% of it budgeted for wafer flatness, about 16 nm over a field. A particle that transfers to the chuck affects later wafers. At larger nodes depth of focus absorbed microns; from 28 nm, fabs inspect the back side before the scanner.
  2. M. Östling, IH2655, lecture 9, "Microlithography," KTH (Spring 2013). R = k1·λ/NA and DOF = k2·λ/NA²; higher-NA lenses decrease the depth of focus. Resist contrast γ = 1 / log10(Df/D0): about 2–3 for DNQ resists, 5–10 for DUV; chemical amplification steepens the transition. Standing waves on reflective layers, suppressed by an anti-reflective coating; post-exposure bake smooths them. Soft bake 90–100 °C; develop 30 s to minutes.