THE COURSE / M4 PATTERNING / M4.7
More than one exposure
After this lesson you can:
- Explain litho-etch-litho-etch, and why overlay limits it.
- Follow self-aligned double and quadruple patterning, and say what sets the final line width.
- Say why spacer-made lines need cuts, and when a layer uses spacers rather than EUV.
Loading the lesson…
Sources
- T. Ihara, T. Hongo, A. Takahashi (Tokyo Institute of Technology) and C. Kodama (Toshiba), "Grid-based Self-Aligned Quadruple Patterning Aware Two Dimensional Routing Pattern," DATE 2016. Under ArF immersion, multiple patterning: litho-etch triple patterning struggles to reach its pitch because of inevitable overlay error. Self-aligned multiple patterning uses a single litho-etch for the mandrel, so there is no misalignment between masks; slimming and sidewall spacers make the fine pitch: once for SADP, twice for SAQP, the mandrel at eight times the final half pitch. The spacers limit the patterns that can be made: fixed widths, loops, no T-shapes; a trim step finishes the pattern.
- S. Hofman, "How immersion lithography saved Moore's Law," ASML (2 August 2023). In 2001 157 nm lithography hit problems; water under the lens extended 193 nm instead, with the same optics, masks and resists. The first immersion system announced in December 2003; volume production in 2006, NA from 0.93 to 1.2; then multi-patterning, where "overlay, rather than imaging resolution, became the critical parameter".
- ASML, TWINSCAN NXT:2050i (product page, read 26 October 2026). A 1.35 NA, 193 nm catadioptric projection lens, production resolution down to 38 nm with dipole illumination and 40 nm with C-quad; a 26 × 33 mm field at 4× reduction; the ORION alignment sensor; a UV level sensor mapping the wafer in line; a new immersion hood that loses less water, improving defects; 295 wafers an hour; 2.5 nm cross-matched overlay with ASML's EUV systems.