Skip to content

THE COURSE / M7 DOPING AND HEAT / M7.5

Diffusion and the spike anneal

After this lesson you can:

  • Say what an anneal after an implant must do, and what it must not.
  • Explain transient enhanced diffusion, and why a cooler anneal can move dopants further than a hotter one.
  • Say why anneals moved from furnaces to lamps and spikes of about a second.

Loading the lesson…

Sources

  1. J. D. Plummer, M. D. Deal and P. B. Griffin, "Diffusion," EE212 class handout for chapter 7 of Silicon VLSI Technology (Stanford, 1999). Where a transistor's doped regions go; predeposition and drive-in against implantation and annealing; Fick's laws, the Gaussian spreading as √(Dt), diffusivities rising exponentially with temperature (boron: D₀ = 1.0 cm²/s, Eₐ = 3.5 eV); successive anneals add their Dt.
  2. J. D. Plummer, M. D. Deal and P. B. Griffin, "Ion Implantation," EE212 class handout for chapter 8 of Silicon VLSI Technology (Stanford, 1999). Doses of 10¹¹ to 10¹⁶ per cm², counted by the integrated beam current; the beamline; a Gaussian with range Rp and straggle ΔRp, peak = dose ÷ (√(2π)·ΔRp); mask thickness; channeling, eased by a 7° tilt; damage, amorphization, regrowth; transient enhanced diffusion.
  3. W. Lerch and J. Niess, "Advancement in Ion Implantation Annealing from Seconds to Milliseconds," invited abstract (SkyLark.Solutions and HQ-Dielectrics). Activation anneals for ultra-shallow source/drain extensions moved from halogen-lamp anneals of seconds to spike anneals of one second, then to flash-lamp and laser anneals of milliseconds; defect annealing always comes with the activation anneal.