Thermal oxidation

After this lesson you can:

  • Say why silicon's own oxide matters, and what growing it costs the wafer.
  • Predict an oxide's growth with the Deal–Grove model: linear while thin, parabolic once thick.
  • Choose dry oxygen or steam, and say what oxidation does to the dopants beneath it.

Loading the lesson…

Sources

  1. J. D. Plummer, M. D. Deal and P. B. Griffin, "Thermal Oxidation," EE212 class handout for chapter 6 of Silicon VLSI Technology (Stanford, 1999). Why silicon's oxide matters; dry and wet oxidation; the Deal–Grove model of 1965, linear then parabolic, with its rate constants; thin oxides grow faster than it predicts; about 2.2 times volume expansion; furnaces; oxidation-enhanced diffusion.
  2. J. D. Plummer, M. D. Deal and P. B. Griffin, "Diffusion," EE212 class handout for chapter 7 of Silicon VLSI Technology (Stanford, 1999). Where a transistor's doped regions go; predeposition and drive-in against implantation and annealing; Fick's laws, the Gaussian spreading as √(Dt), diffusivities rising exponentially with temperature (boron: D₀ = 1.0 cm²/s, Eₐ = 3.5 eV); successive anneals add their Dt.