A millisecond of heat, and choosing

After this lesson you can:

  • Explain how a millisecond anneal heats only the surface, and why it cools so fast.
  • Say why a hotter, shorter anneal activates more dopant for the same diffusion.
  • Choose the implanter and the heat for each doping step, and defend the choice.

Loading the lesson…

Sources

  1. P. Timans, G. Xing, S. Hamm, S. McCoy, J. Cibere, G. Stuart and D. Camm, "Flat-Top Flash Annealing for Advanced CMOS Processing," AVS Joint Thermal Group talk (Mattson Technology, 18 July 2012). Shallow, abrupt source/drain extensions moved from spike to millisecond anneals; under half a second needs heating only the surface, by flash lamps or scanned lasers; boron's activation (about 5 eV) climbs faster with temperature than its diffusion (about 3.5 eV); millisecond anneals up to about 10 ms and 1,300 °C; examples at 2×10¹⁵ per cm², arsenic at 2.5 keV and boron at 1 keV.
  2. W. Lerch and J. Niess, "Advancement in Ion Implantation Annealing from Seconds to Milliseconds," invited abstract (SkyLark.Solutions and HQ-Dielectrics). Activation anneals for ultra-shallow source/drain extensions moved from halogen-lamp anneals of seconds to spike anneals of one second, then to flash-lamp and laser anneals of milliseconds; defect annealing always comes with the activation anneal.
  3. J. D. Plummer, M. D. Deal and P. B. Griffin, "Ion Implantation," EE212 class handout for chapter 8 of Silicon VLSI Technology (Stanford, 1999). Doses of 10¹¹ to 10¹⁶ per cm², counted by the integrated beam current; the beamline; a Gaussian with range Rp and straggle ΔRp, peak = dose ÷ (√(2π)·ΔRp); mask thickness; channeling, eased by a 7° tilt; damage, amorphization, regrowth; transient enhanced diffusion.
  4. L. Rubin and J. Poate, "Ion Implantation in Silicon Technology," The Industrial Physicist 9(3), 12–15 (American Institute of Physics, 2003). Implantation displaced diffusion for being more precise, reliable and repeatable; dose and energy are set on the tool; up to 35 implants in a CMOS chip; three classes of implanter, high current, medium current and high energy, with their beam currents, energies and uses; tilts up to 60°. Both authors worked at Axcelis.