Source, drain, and the gate at last

After this lesson you can:

  • Explain why the source and drain are grown back by epitaxy, doped as they grow.
  • Follow the replacement gate: fill, polish, temporary gate out, channels released, high-k and metal in.
  • Explain what limits the gate between the sheets, and how earlier heat makes the release harder.

Loading the lesson…

Sources

  1. Q. Zhang, Y. Zhang, Y. Luo and H. Yin, "New structure transistors for advanced technology node CMOS ICs," National Science Review 11, nwae008 (2024). Stacked nanosheet transistors: about 80% of the flow shared with a gate-last FinFET, plus four new steps (sub-fin doping, Si/SiGe superlattice epitaxy, inner spacers, channel release); the superlattice grown below 650 °C; inner spacers of more than ten steps; SiGe removed at over 100:1; the sub-fin's leakage and bottom dielectric isolation; wider sheets for more current; the gate between the sheets. FinFETs used from the 22 nm node to 3 nm; fins grown thinner and taller bring reduced mobility, random doping fluctuation and Vt differences, and around 3 nm short-channel effects. GAA nanosheets: better electrostatics than FinFETs, more effective width from stacked sheets, and a broad allowable width for flexible design; Samsung's stacked three-sheet GAAFETs with 12 nm gates; an imec 2016 nanowire with a 24 nm gate reached 65 mV/decade and DIBL of 42 mV/V. Channel doping much reduced in FinFETs and GAAFETs. CFET stacks the n- and p-type transistors vertically, removing the n-to-p spacing, toward cells of four or even three tracks.
  2. M. Wang, X. Guo, Z. Huang, M. Liao, T. Liu et al., "Influence of Device Structure and Manufacturing Thermal Budget on Channel Release Module in GAA NSFET and Process Optimization," Nanomaterials 16, 716 (2026). Channel release by non-plasma gas etching at a SiGe/Si selectivity of up to 87, silicon damage under 1 nm at over 100% overetch; wide and narrow sheets released together; annealing at 500 and 700 °C diffuses germanium, thickening the SiGe from 14.25 to 15.31 nm and slowing its etch; the gate stack's total thickness is fixed by the SiGe grown at the start; several threshold voltages per device type.