Skip to content

THE COURSE / M9 MEASURE AND YIELD / M9.8

Failure analysis

After this lesson you can:

  • Follow a failing die from its test result, through fault isolation, to a cross-section.
  • Explain how a DualBeam cuts a slice for the TEM, and why a protective cap goes on first.
  • Say what the preparation itself can leave behind, and why it matters.

Loading the lesson…

Sources

  1. J.-Y. Bae, K.-S. Lee, H. Hur et al., "3D Defect Localization on Exothermic Faults within Multi-Layered Structures Using Lock-In Thermography," Sensors 17, 2331 (2017). Shorts, junction breakdowns and resistive opens give off local heat; lock-in thermography, pulsing the device and averaging, localizes these faults, with depth from the phase.
  2. V. K. Ravikumar, J. M. Chin, W. Lua et al., "Super-resolution laser probing of integrated circuits using algorithmic methods," Nature Communications 13, 5155 (2022). Laser probing localizes faults by focusing near-infrared light through the silicon substrate onto transistors as diagnostic tests run; with 1064 nm light and a solid immersion lens the resolution is about 180 nm, against transistors of about 55–60 nm at the 7 nm node.
  3. N. T. H. Farr, G. M. Hughes and C. Rodenburg, "Monitoring Carbon in Electron and Ion Beam Deposition within FIB-SEM," Materials 14, 3034 (2021). A deposited layer protects surface features before ion-beam exposure and raises the success rate of TEM lamellae prepared by FIB in semiconductor failure analysis.
  4. N. G. Orji, M. Badaroglu, B. M. Barnes, C. Beitia, B. D. Bunday, U. Celano, R. J. Kline, M. Neisser, Y. Obeng and A. E. Vladár, "Metrology for the next generation of semiconductor devices," Nature Electronics 1, 532–547 (2018), author manuscript. For some products more than half the manufacturing steps can involve measurement; CD-SEM, scatterometry and image-based or scatterometry overlay, CD-SAXS, TEM (destructive), AFM; hybrid metrology; precision and stability matter more than absolute accuracy for most fab uses, traceability when instruments are compared; methods divergence, such as 2.7 nm between CD-AFM and EUV scatterometry; under 5 nm, a deviation under 10% can affect device performance.
  5. C. Chen, L. Gao, J. Jia and Z. Ding, "Focused-Ion-Beam Artifacts and Evidence Reliability in Advanced Microscopy of Energy Materials," Molecules 31, 2148 (2026). FIB creates access by modifying the specimen: ion milling can introduce amorphous layers, implanted ions, redeposited material and local mixing, which can be mistaken for real features.